+74957899228

Plate heat-exchanger limescale protection (dairy)

Before, after 6 months of operation, heat-exchanger’s plates ware covered with lime-scale. It should be opened and clean with chemicals. Now after 90 days of operation, the heat-exchanger plates are clean, like new. No lime-scale traces.

September 29, 2017 by admin 0 Comments Tags: dairy, heat-exchanger
Read More

Testimonial: gates heating heat-exchangers descaling (Russian Railways).

After two months of operation, temperature at the gates heating heat-exchangers output changed from 38-40C to 57-64C (from 100-104F to 135-147F). Deposits amount on the plates of the hot water heat-exchanger significantly decreased in compare with the previous year.

July 03, 2016 by admin 0 Comments
Read More

Testimonial: steam-water heat-exchangers lime-scale protection

After 3 months no new lime-scale were found in heat-exchangers. Residual deposits are softened and can be easily removed.

May 24, 2016 by admin 0 Comments
Read More